| of waterproofing. The existing mortar should be raked out to a depth of at least 50 mm, all loose mortar removed and the joints washed out, repointed with lime mortar and finished with silicone or polysulphide mastic applied by a gun to a depth of about 20 mm. | of waterproofing. The existing mortar should be raked out to a depth of at least 50 mm, all loose mortar removed and the joints washed out, repointed with lime mortar and finished with silicone or polysulphide mastic applied by a gun to a depth of about 20 mm. | ||
| - | {{ :: | + | {{ :: |